Enhancing Critical Cracking Thickness of TiO₂ Films through Evaporation-Driven GME in Non-Volatility Butanediol–Water Mixtures

Authors

  • Juang Bhakti Hastyadi Society of Petroleum Engineers Kuala Lumpur, Society of Petroleum Engineers, Kuala Lumpur, Malaysia Author

DOI:

https://doi.org/10.64229/safkc237

Keywords:

Lyotropic liquid crystal, TiO₂ colloidal film, Critical cracking thickness, 1,4-butanediol, 1-glyceryl monooleyl ether, Non-volatile, Capillary fracture

Abstract

We report a systematic investigation of GME (1-glyceryl monooleyl ether) self-assembly of TiO₂–water–butanediol quaternary colloidal suspensions and its consequences for crack formation during film drying. Because 1,4-butanediol has a boiling point of ~230°C and a vapour pressure orders of magnitude below that of water, drying progressively enriches the GME–butanediol–water phase in both co-solvent and surfactant rather than depleting it of a volatile additive. Cross-polarised optical microscopy (POM) established that lamellar or hexagonal lyotropic liquid-crystalline (LC) phases form at ≥2 wt% GME in butanediol:water 1:20 mixtures, and at ≥2 wt% GME in 3:7 mixtures. UNIFAC-based drying-path simulations confirmed that water evaporates preferentially, predicting that 3:7 BDO/H₂O formulations at ≥2 wt% GME cross into the lamellar LC window when ≈72 ± 4% of the initial water remains. Critical cracking thickness (hᴄᴄᴛ) measurements on TiO₂ films (≈200 nm, 3.5 vol%) demonstrated a 2.3-fold increase from 17.5 ± 0.6 µm (additive-free control) to 41.4 ± 2.9 µm at 3:7 BDO/3 wt% GME at 25°C (p < 0.001, one-way ANOVA). The enhancement is primarily LC-mediated: the apparent shear modulus Gₐₚₚ of the LC phase (exp(0.71ϕf)) elevates the Tirumkudulu–Russel fracture-resistance prefactor by a factor of ≈1.7× (model R² = 0.993). Residual butanediol in dried films (9.4 ± 0.6 wt% at the 3:7/2 wt% GME condition) contributes a secondary plasticisation effect (r² = 0.62 vs. r² = 0.91 for the LC contribution). Isomer comparison confirmed that 1,4-butanediol (hᴄᴄᴛ = 34.0 µm) outperforms 1,3-butanediol (29.7 µm) and 2,3-butanediol (27.2 µm), consistent with the linear backbone geometry of 1,4-BDO favouring GME lamellar packing. These results demonstrate a low-volatility, low-VOC additive route to crack-free thick particulate coatings and offer a mechanistic framework for non-volatile co-solvent–amphiphile systems in particulate film drying.

References

[1]Tirumkudulu MS, Russel WB. Cracking in drying latex films. Langmuir, 2005, 21(11), 4938-4948. DOI: 10.1021/la048298k

[2]Yamamura, M. Hindered cracking in colloidal suspension coatings via evaporation-driven lyotropic liquid crystals. AIChE Journal, 2025, 71(7), e18837. DOI: 10.1002/aic.18837

[3]Barauskas J, Svedaite I, Butkus E, Razumas V, Larsson K, Tiberg F, Synthesis and aqueous phase behavior of 1-glyceryl monooleyl ether. Colloids and Surfaces B: Biointerfaces, 2005, 41(1), 49-53. DOI: 10.1016/j.colsurfb.2004.11.008

[4]Wittig R, Lohmann J, Gmehling J. Vapor-liquid equilibria by UNIFAC group contribution. 6. Revision and extension. Industrial & Engineering Chemistry Research, 2003, 42(1), 183-188. DOI: 10.1021/ie020506l

[5]Griffith AA. The phenomena of rupture and flow in solids. Philosophical Transactions of the Royal Society A, 1921, 221, 163-198. DOI: 10.1098/RSTA.1921.0006

[6]Chiu RC, Garino TJ, Cima MJ. Drying of granular ceramic films: I, effect of processing variables on cracking behavior. Journal of the American Ceramic Society, 1993, 76, 2257-2264.

[7]Engström S, Wadsten-Hindrichsen P, Hernius B. Cubic, sponge, and lamellar phases in the glyceryl monooleyl ether-propylene glycol-water system. Langmuir, 2007, 23(20), 10020-10025. DOI: 10.1021/la701217b

[8]Goehring L, Clegg WJ, Routh AF. Plasticity and fracture in drying colloidal films. Physical Review Letters, 2013, 110(2), 024301. DOI: 10.1103/PhysRevLett.110.024301

[9]Schneider M, Maurath J, Fischer SB, Weiß M, Willenbacher N, Koos E. Suppressing crack formation in particulate systems by utilizing capillary forces. ACS Applied Materials & Interfaces, 2017, 9(12), 11095-11105. DOI: 10.1021/acsami.6b13624

[10]Yamamura M. Adsorption-mediated nonlinearity of critical cracking thickness in drying nanoparticle-polymer suspensions. AIChE Journal, 2021, 67(5), e17229. DOI: 10.1002/aic.17229

[11]Nakajima H, Matsumoto N, Ogura T, Kondo N, Mimura K, Tanaka S, et al. Hidden correlation between rheological dynamics and crack formation in water-based slurry. Journal of the European Ceramic Society, 2024, 44(6), 4141-4149. DOI: 10.1016/j.jeurceramsoc.2023.12.069

[12]Moorhead A, Francis LF. Characterizing stress development and cracking of ceramic particulate coatings during drying. Journal of the American Ceramic Society, 2024, 107, 2837-2848. DOI: 10.1111/jace.19644

[13]Niu ZX, Zhao YP, Zhang QT, Zhao ZY, Ge DT, Zhou JJ, et al. Suppression of cracking in drying colloidal suspensions with chain-like particles. Journal of Chemical Physics, 2024, 160(16), 164901. DOI: 10.1063/5.0203112

[14]Tanaka H, Komoda Y, Horie T, Ohmura N. Stress development of latex coatings in a convection drying with the accumulation and deformation of polymer particles. Progress in Organic Coatings, 2022, 170, 106941. DOI: 10.1016/j.porgcoat.2022.106941

[15]Santanach Carreras E, Chabert F, Dunstan DE, Franks GV. Avoiding "mud" cracks during drying of thin films from aqueous colloidal suspensions. Journal of Colloid and Interface Science, 2007, 313(1), 160-168. DOI: 10.1016/j.jcis.2007.03.076

[16]Koga S, Inasawa S. Packing structures and formation of cracks in particulate films obtained by drying colloid-polymer suspensions,” Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2019, 563, 95-101, 2019. DOI: 10.1016/j.colsurfa.2018.11.066

[17]Oh K, Kim S, Shen Z, Jeong MH, Toivakka M, Lee H. Effect of carboxymethyl cellulose and polyvinyl alcohol on the cracking of particulate coating layers. Progress in Organic Coatings, 2022, 170, 106951. DOI: 10.1016/j.porgcoat.2022.106951

[18]Kozuka H, Takenaka S. Single-step deposition of gel-derived lead zirconate titanate films: Critical thickness and gel film to ceramic film conversion. Journal of the American Ceramic Society, 2002, 85(11), 2696-2702. DOI: 10.1111/j.1151-2916.2002.tb00516.x

[19]Chen Z, Burtovyy R, Kornev K, Luzinov I, Xu D, Peng F. The effect of polymer additives on the critical thicknesses of mullite thin films obtained from the monophasic sol-gel precursors. Journal of Sol-Gel Science and Technology, 2016, 80, 285-296. DOI: 10.1007/s10971-016-4117-x

[20]Qiao J, Adams J, Johannsmann D. Addition of halloysite nanotubes prevents cracking in drying latex films. Langmuir, 2012, 28(23), 8674-8680. DOI:10.1021/la3011597

[21]Singh KB, Deoghare G, Tirumkudulu MS. Cracking in soft-hard latex blends: Theory and experiments. Langmuir, 2009, 25(2), 751-760. DOI: 10.1021/la802857q

[22]Jin Q, Tan P, Schofield AB, Xu L. Eliminating cracking during drying. European Physical Journal E: Soft Matter, 2013, 36(3), 28. DOI: 10.1140/epje/i2013-13028-9

[23]Fischer SB, Koos E. Influence of drying conditions on the stress and weight development of capillary suspensions. Journal of the American Ceramic Society, 2021, 104(3), 1255-1270. DOI: 10.1111/jace.17553

[24]Urase M, Maejima Y, Watanabe T, Kishikawa K, Fudouzi H, Kohri M. Crack-free structural color materials prepared without disrupting the particle arrangement by controlling the internal stress relaxation and interactions of the melanin particles. Langmuir: The ACS journal of surfaces and colloids. 2023, 39(25), 8725-8736.

[25]Badar A, Tirumkudulu MS. Moving cracks in drying colloidal films. Soft Matter, 2022, 18(11), 2252-2275. DOI: 10.1039/d1sm01568k

[26]Uchino T, Murata A, Miyazaki Y, Oka T, Kagawa Y. Glyceryl monooleyl ether-based liquid crystalline nanoparticles as a transdermal delivery system of flurbiprofen: Characterization and in vitro transport. Chemical and Pharmaceutical Bulletin, 2015, 63(5), 334-340. DOI: 10.1248/cpb.c15-00029

[27]SuzukiY, Tsutsumi H. Emulsifying characteristics of α-monoalkyl glyceryl ether. Journal of the Japan Oil Chemists’ Society, 1987, 36, 588-593. DOI: 10.5650/jos1956.36.588

[28]Oka T, Ohta N. Two distinct cylinder arrangements in monodomains of a lyotropic liquid crystalline hexagonal II phase: Monodomains with straight cylinders and ringed cylinders in capillaries. Langmuir, 2016, 32(30), 7613-7620. DOI: 10.1021/acs.langmuir.6b00996

[29]Younus M, Hawley A, Boyd BJ, Rizwan SB. Bulk and dispersed aqueous behaviour of an endogenous lipid, selachyl alcohol: Effect of Tween 80 and Pluronic F127 on nanostructure. Colloids and Surfaces B: Biointerfaces, 2018, 169, 135-142. DOI: 10.1016/j.colsurfb.2018.05.013

[30]Jang E, Koga H, Mawatari Y, Kage H, Yamamura M. Composition-dependent stress oscillations in a dilute suspension under shear. Journal of Chemical Engineering of Japan, 2016, 49, 6-9. DOI: 10.1252/jcej.14we437

[31]Yamamura M. Sigmoidal temporal increase in shear viscosity of titania-toluene-ethanol colloidal suspensions. Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2023, 675, 132047. DOI: 10.1016/j.colsurfa.2023.132047

[32]Yamamura M. Drying paths of phase-separating solution coatings exposed to humidity. Journal of Coatings Technology and Research, 2022, 19, 15-23. DOI: 10.1007/s11998-021-00483-z

[33]Fong C, Le T, Drummond CJ. Lyotropic liquid crystal engineering-ordered nanostructured small molecule amphiphile self-assembly materials by design. Chemical Society Reviews, 2012, 41(3), 1297-1322. DOI: 10.1039/c1cs15148g

[34]Haw MD, Gillie M, Poon WCK. Effects of phase behavior on the drying of colloidal suspensions. Langmuir, 2002, 18(5), 1626-1633. DOI: 10.1021/la0110951

Downloads

Published

2026-09-21

Issue

Section

Articles

How to Cite

Juang Bhakti Hastyadi. (2026). Enhancing Critical Cracking Thickness of TiO₂ Films through Evaporation-Driven GME in Non-Volatility Butanediol–Water Mixtures. Chemical Technology and Engineering Applications, 1(2), 1-19. https://doi.org/10.64229/safkc237